Arcaloy ER316L is a low carbon grade of stainless steel which provides additional corrosion resistance where necessary.
Arcaloy ER316L is a solid wire and is for welding stainless steel Types 316, 316L and in some cases the 200 series stainless steels where strength is not important. In many cases they can also be used for the welding of Types 304 and 304L with some exceptions such as nitric acid service. In the case of the MIG (GMAW), spray, pulse or short-arc modes of transfer are used depending on the gas used. With this process, shielding gases of argon with 1 or 2% oxygen are commonly used for 'spray' and a mixture of 90% helium - 7.5% argon - 2.5% carbon dioxide is used for short-arc.
* This item is subject to Industry Alloy Surcharges

| GTAW using 100% Argon | |
|---|---|
| Yield Stress | 60 ksi, 410 MPa |
| Tensile Strength | 83 ksi, 570 MPa |
| Elongation in 2" | 43 % |
| Impact Toughness at -320ºF (-196ºC) | |
| Lateral Expansion | 40 mils, 1.0 mm |
| GMAW using 98% Argon - 2% O2 | |
| Yield Stress | 60 ksi, 410 MPa |
| Tensile Strength | 82 ksi, 570 MPa |
| Elongation in 2" | 41 % |
| Impact Toughness at -320ºF (-196ºC) | |
| Lateral Expansion | 20 mils, 0.5 mm |
| Typical Chemical Analysis | |
| C | 0.017 % |
| Mn | 1.6 % |
| Si | 0.4 % |
| S | 0.007 % |
| Cr | 18.5 % |
| Ni | 12 % |
| Mo | 2.4 % |
| Cu | 0.2 % |
| Ferrite | 8 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 256071135 | AB ER316L 5/32X36X10T/30CT INK | 662303075248 |
| 259602282 | AB ER316L 3/32X18X10#CT F1 | 662303521608 |
| 256071051 | AB ER316L 1/16X36X10T/30CT INK | 662303044657 |
| 256071069 | AB ER316L 3/32X36X10T/30CT INK | 662303030827 |
| 256071077 | AB ER316L 1/8X36X10T/30CT INK | 662303030834 |
| 257061820 | AB ER316L 1/8X60#CL | 662303027322 |
| 257063321 | AB ER316L 3/32X60#CL | 662303008499 |
| 257065326 | AB ER316L 5/32X60#CL | 662303027339 |
| 257071233 | AB ER316L 045X10#PSP/60CT | 662303043346 |
| 258061118 | AB ER316L 1/16X33#PSP | 662303027742 |
| 258063023 | AB ER316L 030X10#PSP/60CT | 662303027704 |
| 258063031 | AB ER316L 030X33#PSP | 662303047078 |
| 258063510 | AB ER316L 035X33#BAWS | 662303027728 |
| 258064518 | AB ER316L 045X33#BAWS | 662303027735 |
| 258065523 | AB ER316L 035X10#PSP/60CT | 662303027865 |
| 258065523-03 | AB ER316L 035X10#PSP/60CT | 662393014080 |
| 258075522 | AB ER316L 035X10#PSP/60CT | 662393012291 |
| 259600559 | AB ER316L 1/16X36X10#CT F1 | 662303519254 |
| 259601177 | AB ER316L 1/16X18X10#CT F1 | 662303667917 |
| 259601516 | AB ER316L 1/8X36X10#CT F2 | 662303520045 |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr |
| .035 in., 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr |
| .045 in., 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in., 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in., 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in., 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.