OK Tigrod 316LSi is a bare, corrosion-resistant, austenitic stainless for welding 316 steels. This high silicon Tigrod improves the wetting characteristics of the weld deposit.
OK Tigrod 316LSi is a bare, corrosion-resistant, chromium-nickel-molybdenum rod for welding of austenitic stainless alloys of 18% Cr - 8% Ni and 18% Cr - 10% Ni - 3% Mo types. OK Tigrod 316LSi has a good general corrosion resistance, in particular the alloy has very good resistance against corrosion in acid and chlorinated environments. The alloy has a low carbon content which makes it particularly recommended where there is a risk of intergranular corrosion.
* This item is subject to Industry Alloy Surcharges

| Yield Strength | 70 ksi, 480 MPa |
|---|---|
| Tensile Strength | 91 ksi, 630 MPa |
| Elongation in 2" | 33 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -76°F (-60°C) | 81 ft.-lbs, 110 J |
| Testing Temperature -320ºF (-196ºC) | 81 ft.-lbs., 110 J |
| Testing Temperature 68ºF (20ºC) | 103 ft.-lbs., 140 J |
| Typical wire analysis | |
| C | <0.03 % |
| Mn | 1.8 % |
| Si | 0.8 % |
| Cr | 19.0 % |
| Ni | 12.5 % |
| Mo | 2.8 % |
| Cu | <0.3 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 163216R15A | ES OK ER316LSI 1/16X39X11 E2 | 000000000000 |
| 163224R15A | ES OK ER316LSI 3/32X39X11 E2 | 000000000000 |
| 163232R15A | ES OK ER316LSI 1/8X39X11 E2 | 000000000000 |
| 163240R15A | ES OK ER316LSI 5/32X39X11 E2 | 000000000000 |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.