Print this page

ARCALOY ER317L

Arcaloy 317L is a continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding of austenitic stainless alloys of 19% Cr, 13% Ni, 3% Mo types. Arcaloy 317L can be used in combination with OK Flux 10.93 or 10.94.

Features

Arcaloy ER317L produces a low carbon analysis and was developed to weld type 317 and 317L stainless steel. The additional molybdenum is present to prevent pitting corrosion.

* This item is subject to Industry Alloy Surcharges

ARCALOY ER317L
  • Industry
  • General Fabrication
  • Process
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 6
    • ASME II SFA 5.9 ER317/317L
    • AWS A5.9; ER317/317L

Properties

Typical Properties
C 0.015 %
Mn 1.5 %
Si 0.45 %
Cr 19 %
Ni 14 %
Mo 3.5 %
Cu 0.1 %
Ferrite 7 FN

Part No.

ER317L
Part No. Model / Product Description UPC
257071514 AB ER317L 045X33#BAWS 662393012093
257071522 AB ER317L 1/16X36X10T/30CT INK 662393012116
257071530 AB ER317L 3/32X36X10T/30CT INK 662303049188
257071548 AB ER317L 1/8X36X10T/30CT INK 662303049195
257071555 AB ER317L 035X33#BAWS 662393012109

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in, 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in, 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in, 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in, 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Volts DCEP (Electrode Positive) Deposition Rate
.030 in, 0.8 mm 156-312 ipm, 396-792 cm/min 15-20 40-120 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr.
.035 in, 0.9 mm 156-312 ipm, 396-792 cm/min 15-21 60-140 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 17-22 100-210 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.

Extra Info

Arcaloy ER317L is a solid wire and is for welding stainless steel Types 317, 317L. In many cases they can also be used for the welding of Types 316 and 316L where greater corrosion resistance is required in the weld metal. Depending upon its form, Arcaloy ER317L can be used in the MIG, TIG or submerged arc processes to name the three most common. In the case of the MIG (GMAW), spray, pulse or short-arc gases of argon with 1 or 2% oxygen are commonly used for 'spray' and a mixture of 90% helium - 7.5 argon - 2.5 carbon dioxide is used for 'short-arc'. For TIG (GTAW), 100% argon or argon with some helium additions are used. A flux, such as OK Flux 10.93, is used with the larger sizes of Arcaloy ER317L for submerged-arc welding.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.