ARCALOY ER320LR

Arcaloy ER320LR Tigrod is designed for welding Carpenter 20Cb-3® type stainless steels.

Features

The low residual content compared to ER320 gives increased crack resistance. The interpass temperature and stresses should be kept low. Arcaloy ER320LR is only available in GTAW rod form where the shielding gas used is 100% argon or argon with some helium additions.

* This item is subject to Industry Alloy Surcharges

ARCALOY ER320LR
  • Industry
  • Process
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER320LR
    • ASME II SFA 5.9 ER320LR
    • ASME IX F No. 6

Properties

Typical Properties
GTAW using 100% Argon  
Yield Stress 57 ksi, 400 MPa
Tensile Strength 81 ksi, 560 MPa
Elongation in 2" 37 %
Typical Chemical Analysis  
C 0.007 %
Mn 1.8 %
Si 0.05 %
Cr 20 %
Ni 33 %
Mo 2.4 %
Cu 3.4 %
Nb 0.25 %
Ferrite 0 FN

Part No.

ER320LR
Part No. Model / Product Description UPC
256071457 AB ER320LR 1/16X36X10#T/30 INK 662303073282
256071465 AB ER320LR 3/32X36X10#T/30 INK 662303073299
256071473 AB ER320LR 1/8X36X10#T/30 INK 662303073305

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.