Arcaloy ER347 is a columbium stabilized stainless steel for welding types 347 and 321 stainless, comes in MIG, TIG, and SAW forms.
Arcaloy ER347 is a solid wire and is for welding stainless steel Types 304, 321 and 347. It may be successfully used for the welding of Types 304L although Arcaloy ER308L is usually the choice. All 347 filler metals should not be used in service under creep conditions (high stress & high temperature combined). Depending upon its form, Arcaloy ER347 can be used in the MIG, TIG or submerged arc processes to name the three most common.
In the case of the MIG (GMAW), spray, pulse or short-arc modes of transfer are used depending on the gas used. With this process, shielding gases of argon with 1 or 2% oxygen are commonly used for 'spray' and a mixture of 90% helium - 7.5% argon - 2.5% carbon dioxide is used for 'short-arc'. There is likely to be some loss of niobium with submerged arc welding.
Arcaloy ER347 is designed for welding types 321 and 347, when the service temperature is below 600°F (316°C). Used where service conditions require maximum resistance to corrosion.
* This item is subject to Industry Alloy Surcharges

| GTAW using 100% Argon | |
|---|---|
| Yield Stress | 65 ksi, 450 MPa |
| Tensile Strength | 100 ksi, 690 MPa |
| Elongation in 2" | 45 % |
| Typical Chemical Analysis | |
| C | 0.03 % |
| Mn | 1.5 % |
| Si | 0.4 % |
| Cr | 19.5 % |
| Ni | 9.5 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Nb | 0.5 % |
| Ferrite | 10 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 258093525 | AB ER347 035X33#PSP | 662303076597 |
| 256073156 | AB ER347 1/16X36X10T/30CT INK | 662303049201 |
| 256073164 | AB ER347 3/32X36X10T/30CT INK | 662303049218 |
| 256073172 | AB ER347 1/8X36X10T/30CT INK | 662303049225 |
| 258091115 | AB ER347 1/16X33#PSP | 662303027919 |
| 258093517 | AB ER347 035X33#BAWS | 662303027896 |
| 258094515 | AB ER347 045X33#BAWS | 662303027902 |
| 259600807 | AB ER347 1/16X36X10#CT F2 | 662303522711 |
| 259601672 | AB ER347 1/8X36X10#CT F2 | 662303519766 |
| 259601680 | AB ER347 1/8X36X10#CT F1 | 662303030032 |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr |
| .035 in., 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr |
| .045 in., 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in., 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in., 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in., 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |