Print this page

ESAB ER308LSi MIG

ESAB ER308LSi MIG is a silicon enhanced MIG wire which significantly increases wetting action, resulting in a smooth weld to improve weldability and performance on 304 steels.

Features

ESAB ER308LSi MIG is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18 Cr- 8% Ni type. The alloy has a low carbon content, making it particularly recommended where there is a risk of intergranular corrosion.

* This item is subject to Industry Alloy Surcharges

Arcaloy ER308LSi
  • Industry
  • General Fabrication
  • Automotive
  • Process
  • Food and Beverage
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • ASME II SFA 5.9 ER308Si/308LSi
    • ASME IX F No. 6
    • Certified by CWB - AWS A5.9
    • AWS A5.9; ER308Si/ER308LSi

Properties

Typical Properties
GMAW using 98% Argon / 2% Oxygen  
Yield Stress 55 ksi, 380 MPa
Tensile Strength 85 ksi, 690 MPa
Elongation in 2" 40 %
Typical Chemical Analysis  
C 0.015 %
Mn 1.7 %
Si 0.8 %
S 0.01 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.2 %
Ferrite 10 FN

Part No.

ER308LSi
Part No. Model / Product Description UPC
161208982A ES OK ER308LSI 030X33#BAWS 000000000000
161209932A ES OK ER308LSI 035X550#OMP 000000000000
161209982A ES OK ER308LSI 035X33#BAWS 662303082833
161211982A ES OK ER308LSI 045X33#BAWS 662303079871
161216982A ES OK ER308LSI 1/16X33#BAWS 000000000000
161211932A ES OK ER308LSI 045X550#OMP 662303076849
258123140 AB ER308LSI 035X500#OMP 662303667733
258123538 AB ER308LSI 045X500#OMP 662303667634
258121110 AB ER308LSI 1/16X33#PSP 662303027520
258123025 AB ER308LSI 030X10#PSP/60CT 662303027483
258123116 AB ER308LSI 030X33#PSP 662303027506
258123157 AB ER308LSI 035X250#OMP 2/PLT 662303523589
258123306 AB ER308LSI 030X2#4 SP/40#CT 662393013304
258123512 AB ER308LSI 035X33#BAWS 662303027513
258123975 AB ER308LSI 045X250#OMP 2/PLT 662303667726
258124510 AB ER308LSI 045X33#BAWS 662303026387
258125525 AB ER308LSI 035X10#PSP/60CT 662303027490
257011163 AB ER308LSI 023X10#PSP  

SAW

Accessories

Depositions/Paramaters

Short Circuit Transfer Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.030 in., 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg/hr
.035 in., 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg/hr
.045 in., 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg/hr
Spray Arc Transfer Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.030 in., 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg/hr
.035 in., 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg/hr
.045 in., 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg/hr
.062 in., 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg/hr

Extra Info

Complementary Products

Seismic Data