Print this page

ARCALOY ER409Nb

Arcaloy ER409Nb is a ferritic stainless steel stabilized with Niobium for joining 409 stainless.

Features

Arcaloy ER409Nb is a stabilized ferritic grade bare wire that offers superior properties on 409 grade steels. This alloy offers resistance to corrosion for applications requiring such properties.

* This item is subject to Industry Alloy Surcharges

ARCALOY ER409Cb
  • Industry
  • Automotive
  • Welding Process
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER409Nb

Properties

Typical Properties
C 0.03 %
Mn 0.45 %
Si 0.5 %
P 0.02 %
S 0.01 %
Cr 11 %
Ni 0.3 %
Mo 0.1 %
Cu 0.1 %
Nb 0.35 %

Part No.

ER409Nb
Part No. Model / Product Description UPC
256196437 AB ER409NB 035X33#PSP 662303071141
256196452 AB ER409NB 045X33#PSP 662303071165
258080225 AB ER409NB 035X250#OMP 662303667887
258080233 AB ER409NB 045X250#OMP 662303667702

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in, 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in, 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in, 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in, 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Volts DCEP (Electrode Positive) Deposition Rate
.030 in, 0.8 mm 156-312 ipm, 396-792 cm/min 15-20 40-120 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr.
.035 in, 0.9 mm 156-312 ipm, 396-792 cm/min 15-21 60-140 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 17-22 100-210 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.