OK Autrod 2209

Features

A continuous, solid, corrosion-resistant, duplex wire for the GMA welding of austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. OK Autrod 2209 (''Duplex'') has high general corrosion resistance. In media containing chloride and hydrogen sulphide, the alloy has high resistance to intergranular, pitting and especially stress corrosion. The alloy is used in a variety of applications across all industrial segments. OK Autrod 2209 is usually welded with Ar/(1-3%) O2 as the shielding gas.

Former name of this product was OK Autrod 16.86

* This item is subject to Industry Alloy Surcharges

OK Autrod 2209
  • Industry
  • Process
  • Petrochemical
  • Power Generation
  • General Fabrication
  • Pipeline
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER2209

Properties

Typical Properties
Yield Strength 87 ksi, 600 MPa
Tensile Strength 110 ksi, 765 MPa
Weld Metal Hardness, a.w. 240 HB
Elongation in 2" 28 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -4°F (-20°C) 63 ft.-lbs, 85 J
Testing Temperature -76°F (-60°C) 44 ft.-lbs, 60 J
Testing Temperature 68ºF (20ºC) 73 ft.-lbs., 100 J
Typical Undiluted Weld Metal Analysis  
C <0.03 %
Mn 1.7 %
Si 0.5 %
Cr 22.5 %
Ni 8.5 %
Mo 3.3 %
N 0.15 %
Ferrite 45 FN

Part No.

Autrod 2209
Part No. Model / Product Description UPC
1686240300 ES OK 16.86 2.4X25KG CL 662303078478
1686109820 ES OK ER2209 1.0X15KG SP 662303071943
168624R150 ES OK ER2209 2.4X1000X5KG CT 662303070618
168632R150 ES OK ER2209 3.2X1000X5KG CT 662303070625
1686129820 ES OK ER2209 1.2X15KG SP 662303085605

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in, 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in, 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in, 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in, 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Volts DCEP (Electrode Positive) Deposition Rate
.030 in, 0.8 mm 156-312 ipm, 396-792 cm/min 15-20 40-120 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr.
.035 in, 0.9 mm 156-312 ipm, 3.96-792 cm/min 15-21 60-140 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 17-22 100-210 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.

Extra Info