Dual Shield 710X-M

Dual Shield 710X-M is an all-position flux cored wire for general purpose welding.

Features

Dual Shield 710X-M provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 710X-M is designed to be used with 75/25 Argon CO2 gas mix, however pure CO2 may also be used.

Dual Shield 710X-M - Web Image - Medium
  • Industry
  • Barges
  • Shipbuilding
  • Civil Construction
  • Rail Road Car
  • Light Equipment
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • Seismic Certified "D"
    • ASME SFA 5.20
    • CERTIFIED BY C.W.B.- CSA W48
    • ABS
    • AWS A5.20; E71T-1C/T-9C
    • AWS A5.20; E71T-1M-D/T-9M-D

Properties

Typical Properties
As Welded  
Shielding Gas 75 Ar / 25 CO2
Yield Strength 74 ksi, 510 MPa
Tensile Strength 83 ksi, 570 MPa
Elongation (In 2", 51 mm) 29 %
As Welded  
Shielding Gas CO2
Yield Strength 68 ksi, 470 MPa
Tensile Strength 77 ksi, 530 MPa
Elongation (In 2", 51 mm) 30 %
Typical Charpy V-Notch Impact Properties  
Shielding Gas 75 Ar / 25 CO2
Testing Temperature  
0°F (-18°C) 72 ft. - lbs., 97 J
-20°F (-29°C) 56 ft. - lbs., 76 J
Shielding Gas CO2
Testing Temperature  
0°F (-18°F) 60 ft. - lbs., 81 J
-20°F (-29°C) 33 ft. - lbs., 45 J
Typical Undiluted Weld Metal Analysis (%)  
Shielding Gas 75 Ar / 25 CO2
C 0.04
Mn 1.3
Si 0.5
P 0.012
S 0.008
Shielding Gas CO2
C 0.04
Mn 1.0
Si 0.3
P 0.012
S 0.008

Part No.

710X-M
Part No. Model / Product Description UPC
245019831 DS 710X-M 1/16x60#CL  
245019807 DS 710XM 045X33#AWS 662303085063
245019815 DS 710XM 052X33#AWS 662303085070
245019823 DS 710XM 1/16X33#AWS 662303085087

SAW

Accessories

Depositions/Paramaters

Deposition Table Gas: 75/25
Diameter Amperage Voltage Wire Feed Speed Deposition TTW
.045 in. 110 A 19.0 V 150 ipm 2.8 0.625
240 A 26.5 V 450 ipm 11.5 0.625
.052 in. 125 A 20.0 V 125 ipm 3.0 0.75

Extra Info

Shielding Gas

Recommended Shielding Gas: 75% Ar - 25% CO2; however, pure CO2 may also be used

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.