Atom Arc 7018 Acclaim

This newest addition to the family offers the deep, penetrating arc and tough mechanical properties of the original Atom Arc 7018 with greater puddle control.

Features

This newest addition to the family offers the deep, penetrating arc and tough mechanical properties of the original Atom Arc 7018 with greater puddle control resulting in ease of use in out-of-position welding applications and superior arc initiation desired by many newer welders. Both novice and seasoned welders can appreciate its excellent weld performance, wide operating range and easy clean up.


Features


* Greater puddle control resulting in easier out-of-position welds

* Superior arc initiation

* Ease of use with wider operating range and minimal clean-up

* E7018H4R Classification

Atom Arc 7018 Acclaim - Web Image - Medium
  • Industry
  • Shipbuilding
  • Bridge Construction
  • Mobile Machinery
  • Civil Construction
  • General Fabrication
  • Automotive
  • Rail Road Car
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • Mil-E-22200/1 Mil-7018
    • AWS A5.1; E7018H4R
    • ASME SFA 5.1
    • A.B.S.- 2Y / AWS A5.1; E7018
    • D.N.V.- 3Y(H10)
    • L.R.- 3m,3Ym(H10)
    • CERTIFIED BY C.W.B.- CSA W48

Properties

Typical Properties
Yield Strength 65 ksi, 450 MPa
Tensile Strength 79 ksi, 550 MPa
Elongation % in 2" 36 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (29°C) 170 ft-lbs, 230 J
Typical Undiluted Weld Metal Analysis  
C 0.05 %
Mn 1.20 %
Si 0.45 %
P 0.011 %
S 0.008 %

Part No.

Atom Arc 7018 Acclaim
Part No. Model / Product Description UPC
255012007 7018 Acclaim 3/32 x 14 x 50# HSC 662303084646
255012015 7018 Acclaim 1/8x 14 x 50# HSC 662303084134
255012023 7018 Acclaim 5/32 x 14 x 50# HSC 662303085209
255012080 7018 Acclaim, 3/32 x 14 x 5# VALP  
255012049 7018 Acclaim, 3/32 x 14 x 10# HSC  
255012098 7018 Acclaim, 1/8 x 14 x 5# VALP  
255012056 7018 Acclaim 1/8x 14 x 10# HSC  
255012106 7018 Acclaim, 5/32 x 14 x 5# VALP  
255012064 7018 Acclaim, 5/32 x 14 x 10# HSC  
255012072 7018 Acclaim, 3/16 x 14 x 10# HSC  
255012031 7018 Acclaim, 3/16 x 14 x 50# HSC  

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Optimal Amperage Range Amperage Deposition Rate (lbs/hr) Deposition Efficiency
3/32 " 90 70-100 1.7 66.3 %
1/8 " 120 90-160 2.6 71.6 %
140 90-160 2.7 70.9 %
5/32 " 140 130-220 3.1 75 %
170 130-220 3.8 73.5 %
3/16 " 200 200-300 4.9 76.4 %
250 200-300 5.4 74.6 %
7/32 " 250 250-350 6.5 75 %
300 250-350 7.2 74 %
1/4 " 300 300-400 7.7 78 %
350 300-400 8.7 77 %