Print this page

Covered Electrodes - Carbon / Low Alloy Steel

Atom Arc electrodes have set the benchmark for others to follow for over a half century. Performance is the key reason that Sureweld and Atom Arc covered electrodes are selected for high production radiographic welds meeting the strictest mechanical properties. Both lines are tested in accordance with various AWS classifications and conform to strict Military specifications

Carbon Steel

The Sureweld line includes a variety of chemical formulations for high quality welding in mild steel and pipe applications. All Sureweld electrodes are manufactured to strict quality standards and AWS specifications.

Low Hydrogen

Atom Arc was the original low hydrogen electrode and still sets the standard today. Manufactured in a strict quality-controlled environment and tested in strict accordance with AWS standards, Alloy Rods moisture-resistant low hydrogen electrodes deliver consistent performance and x-ray quality weldments.

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.