Covered Electrodes - Stainless Steel

For the welder, an Arcaloy electrode deposit meets the quality control standards and produces results that he can be proud of. These premium electrodes available in a wide variety of alloys are manufactured in an ASME certified quality assurance system that insures the product meets the most rigid metallurgical, chemical and engineering solutions.

E308 (Arcaloy 308L-15)
E308 (Arcaloy 308L-15)

Arcaloy 308L-15 was developed for welding 304L stainless.

E308 (Arcaloy 308L-16)
E308 (Arcaloy 308L-16)

Arcaloy 308L-16 was developed for welding 304L stainless.

E308 (Arcaloy 308/308H-15)
E308 (Arcaloy 308/308H-15)

Arcaloy 308/308H-15 is for welding types 304H and 347H stainless when high temperature service is required.

E308 (Arcaloy 308/308H-16)
E308 (Arcaloy 308/308H-16)

Arcaloy 308/308H-16 was developed for welding types 304H and 347H stainless when high temperature service is required.

E308 (Arcaloy Plus 308L-17)
E308 (Arcaloy Plus 308L-17)

Arcaloy 308L Plus electrode utilize a heavy coating to maximize performance in the flat and horizontal position.

E309 (Arcaloy 309L-15)
E309 (Arcaloy 309L-15)

Arcaloy 309L-15 is used primarily in the overlay of steel or to join stainless steel to carbon or low alloy steels. Best used out-of-position on DC current only.

E309 (Arcaloy 309L-16)
E309 (Arcaloy 309L-16)

Arcaloy 309L-16 is used primarily in the overlay of steel or to join stainless steel to carbon or low alloy steels. Usable on AC or DC current.

E309 (Arcaloy 309/309H-15)
E309 (Arcaloy 309/309H-15)

Arcaloy 309/309H-15 is used for welding type 309 when high temperature service is required. Best used out-of-position on DC current.

E309 (Arcaloy 309/309H-16)
E309 (Arcaloy 309/309H-16)

Arcaloy 309/309H-16 is used for welding type 309 base metal when high temperature service is required. Usable on AC or DC current.

E309 (Arcaloy Plus 309L-17)
E309 (Arcaloy Plus 309L-17)

Arcaloy 309L-17 Plus electrodes utilize a heavy coating to maximize performance in the flat and horizontal position. Usable on AC or DC current.

E309 (Arcaloy 309MoL-15)
E309 (Arcaloy 309MoL-15)

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Best used out-of-position on DC current.

E309 (Arcaloy 309MoL-16)
E309 (Arcaloy 309MoL-16)

Arcaloy 309MoL-16 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Usable on AC or DC current.

E309 (Arcaloy 309Nb-16)
E309 (Arcaloy 309Nb-16)

Arcaloy 309Nb-16 was developed to control carbide precipitation in this type of alloy. Usable on AC or DC current.

E309 (Arcaloy 309Nb-15)
E309 (Arcaloy 309Nb-15)

Arcaloy 309Nb-15 was developed to inhibit carbide precipitation in this type of alloy. Best used out-of-position on DC current.

E310 (Arcaloy 310-15)
E310 (Arcaloy 310-15)

Arcaloy 310-15 electrodes were developed for the welding of type 310 stainless steel. Best used out-of-position on DC current.

E310 (Arcaloy 310-16)
E310 (Arcaloy 310-16)

Arcaloy 310-16 electrodes were developed for the welding of type 310 stainless steel. Usable on AC or DC current.

Arcaloy 312-15 electrodes were originally designed for welding of high tensile alloys to high temperature heat-resisting alloys. Best used out-of-position on AC or DC current.

E312 (Arcaloy 312-16)
E312 (Arcaloy 312-16)

Arcaloy 312-16 electrodes were originally designed for welding of high tensile alloys to high temperature heat-resisting alloys. Usable on AC or DC current.

E316 (Arcaloy 316LF5-16)
E316 (Arcaloy 316LF5-16)

Arcaloy 316LF5-16 is an electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. Designed to weld type 316, 316L steels. Usable on AC or DC current.

E316 (Arcaloy 316LF5-15)
E316 (Arcaloy 316LF5-15)

Arcaloy 316LF5-15 is an electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. Designed to weld type 316, 316L steels. Best used out-of-position on DC current.

E316 (Arcaloy 316/316H-16)
E316 (Arcaloy 316/316H-16)

Arcaloy 316/316H-16 can be used in applications where 316 stainless needs improved due to higher service temperatures. Usable on AC or DC current.

Arcaloy 316/316H-15 can be used in applications where 316 stainless needs improved due to higher service temperature. Best used out-of-position on DC current.

E316 (Cryoarc 316L-15)
E316 (Cryoarc 316L-15)

Cryoarc 316L-15 is a covered electrode designed for low temperature cryogenic applications. Pre-test lot controlled formulation to maximize mechanical properties. Best used out-of-position on DC current.

E316 (Arcaloy Plus 316L-17)
E316 (Arcaloy Plus 316L-17)

Arcaloy 316L-Plus electrode utilizes a heavy coating to maximize performance in the flat and horizontal position. Usable on AC or DC current.

E317 (Arcaloy 317L-15)
E317 (Arcaloy 317L-15)

Arcaloy 317L-15 electrodes are recommended for welding type 317 and 317L. The addition of molybdenum improves the weld metal crack resistance. Best used out-of-position on DC current.

E317 (Arcaloy 317L-16)
E317 (Arcaloy 317L-16)

Arcaloy 317L-16 electrodes are recommended for welding type 317 and 317L. The addition of molybdenum improves the weld metal crack resistance. Usable on AC or DC current.

E320 (Arcaloy 320LR-16)
E320 (Arcaloy 320LR-16)

Arcaloy 320LR-16 is a covered electrode designed to resist hot cracking on Carpenter No.20 Cb-3 steel. Usable on AC or DC current.

E347 (Arcaloy 347-16)
E347 (Arcaloy 347-16)

Arcaloy 347-16 electrodes are especially designed for welding types 347 and 321 alloys. Usable on AC or DC current.

E347 (Arcaloy 347-15)
E347 (Arcaloy 347-15)

Arcaloy 347-15 electrodes are especially designed for welding types 347 and 321 alloys. Best used out-of-position on DC current.

E410 (Arcaloy 410NiMo-16)
E410 (Arcaloy 410NiMo-16)

Arcaloy 410 NiMo-16 is designed for the welding of CA-6NM castings. Usable on AC or DC current.

E410 (Arcaloy 410-16)
E410 (Arcaloy 410-16)

Arcaloy 410-16 electrodes are recommended for welding type 410 straight chromium steel. Usable on AC or DC current.

Duplex (OK 67.50)
Duplex (OK 67.50)

ESAB OK 67.50 is an E2209-17 heavy-coated duplex covered electrode for flat & horizontal position welding. The heavy coating is designed to maximize performance on either AC or DC current.

Duplex (OK 67.55)
Duplex (OK 67.55)

OK 67.55 is an E2209-15 coated electrode specially designed for the welding of duplex stainless steel. The deposited weld metal gives very high ductility down to -45°F/-51°F. Best used out-of-position on DC current.