Low alloy wires provide exceptional weld strength for demanding applications, including fabrication of construction equipment, tanks, submarines, ships and stuctural support elements.
Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as-welded and stress-relieved conditions. Spoolarc 83 is typically used on heavy equipment and high strength piping.
Spoolarc 75 is a MIG and submerged arc wire with 1% nickel content that meets the weathering requirements of AWS D1.1 and D1.5.
Spoolarc 120 is designed to weld high strength, quenched and tempered steels.
TIGROD ER80S-B2 is an ER80S-B2 TIG rod that is used for welding steels such as 0.5% Cr -0.5% Mo, 1% Cr - 0.5% Mo, and 1.25% Cr - 0.5% Mo.
ER80S-B8 is a solid wire for TIG welding requiring creep strength. This 9% chromium - 1% Molybdenum TIG rod is used to weld 9% chromium - 1% Molybdenum steels (ASTM Section IX, P No 5B, Group 1) such as ASTM A335 Grade P9 or ASTM A213 Grade T9. Tigrod products are embossed on opposite ends with the alloy identification.
TIGROD ER90S-B3 is an ER90S-B3 TIG rod that is used to weld 2.5% Cr - 1% Mo steels.
Tigrod ER90S-B9 is designed for high temperature creep resistance on steels up to 9%Cr - 1% Mo(modified grades).
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.