These Coreweld products are ideal for single or multipass welding of low alloy, high strength steels.
This electrode has a high percentage of iron powder resulting in a high efficiency wire with only small islands of slag on the weld deposit.
Coreweld 80CNil is a metal cored wire designed for applications where good impact toughness is required.
Coreweld 110 is a metal cored electrode designed for single and multipass welding of high strength low alloy steels, such as T-1, HY-80, and HY-100.
Coreweld W is a metal cored wire designed for single or multipass welding on weathering grade steels.