Gas-Shielded Metal Core

Arcaloy composite metal cored wires are high efficiency products that deposit at a rate higher than comparable solid wires.

Arcaloy MC316L (EC316L/EC316)
Arcaloy MC316L (EC316L/EC316)

Arcaloy MC316L was developed to maximize welding productivity and reduce the cast to deposit. The alloying elements are designed to improve corrosion resistance on 316 and 316L steels.

Arcaloy MC309LMo (EC309LMo)
Arcaloy MC309LMo (EC309LMo)

Arcaloy MC309LMo was developed to maximize welding performance and reduce the cast to deposit. The alloying elements make it ideal for cladding or joining stainless to low alloy steels.

Arcaloy MC309L (EC309L/EC309)
Arcaloy MC309L (EC309L/EC309)

Arcaloy MC309L was developed to maximize welding performance and reduce the cast to deposit. The alloying elements make it ideal for joining stainless to mild or carbon steels.

Arcaloy MC308L (EC308L/EC308)
Arcaloy MC308L (EC308L/EC308)

Arcaloy MC308L was developed to maximize performance and reduce the cast to deposit. The alloying elements make it ideal for joining 304 or 304L stainless.

Arcaloy MC409Ti (EC409)
Arcaloy MC409Ti (EC409)

Arcaloy MC409Ti is a ferritic metal cored wire developed for welding similar ferritic steels requiring 11-12% Cr. The addition of Titanium (Ti) helps to optimized arc stability and improve weld metal transfer.

Arcaloy MC409Nb (EC409Nb)
Arcaloy MC409Nb (EC409Nb)

Arcaloy 409Nb is a ferritic metal cored wire developed for welding similar ferritic steels requiring 11-12% Cr. The addition of Niobium (Nb) helps optimize weld metal transfer.

Arcaloy MC18CrCb (No AWS Class)
Arcaloy MC18CrCb (No AWS Class)

Arcaloy MC18CrCb is a ferritic metal cored wire developed for welding similar ferritic steels requiring 18-19% Cr. The addition of Niobium (Nb) helps optimize weld metal transfer.

Arcaloy MC430LCb (No AWS Class)
Arcaloy MC430LCb (No AWS Class)

Arcaloy 430LCb is a ferritic metal cored wire developed for welding similar ferritic steels requiring 16-17% Cr. The addition of Niobium (Nb) or Columbium (Cb) optimizes weld metal transfer.

Arcaloy MC439Ti (No AWS Class)
Arcaloy MC439Ti (No AWS Class)

Arcaloy MC439Ti is a ferritic metal cored wire developed for welding similar ferritic steels requiring 16-17% Cr. The addition of Titanium (Ti) optimizes weld metal transfer.

Alloy Shield 423L
Alloy Shield 423L

Alloy Shield 423L is a tubular, composite metal cored wire designed for hard surfacing worn steel mill concast rolls. It produces 35-40 Rc hardness after heat treatment. Used in combination with 601 flux.

Alloy Shield 410NiMo
Alloy Shield 410NiMo

Alloy Shield 410NiMo is a tubular, composite metal cored wire designed for welding CA-6NM castings or other similar Martensitic steels. Used in combination with 10.93 flux.

Arcaloy MC410NiMo (EC410NiMo)
Arcaloy MC410NiMo (EC410NiMo)

Arcaloy MC410NiMo is a martensitic metal cored wire for weld type CA-6NM castings to maximize welding performance and reduce the cast to deposit.

Arcaloy MC410 (EC410)
Arcaloy MC410 (EC410)

Arcaloy MC410 is a Martensitic metal cored wire for welding similar martensitic steels. Developed to maximize welding performance and reduce the cast to deposit.