Print this page

Carbon Steel - Gas-Shielded Flux Core

The Dual Shield line offers the broadest variety of gas shielded flux core wires and electrodes for carbon steel welding available on the market today.

Dual Shield 111-AC (70T-1)
Dual Shield 111-AC (70T-1)

Dual Shield 111-AC is a flux cored wire for single or multipass operation on mild steel and on some low alloy steels.

Dual Shield 111-RB (70T-1)
Dual Shield 111-RB (70T-1)

Dual Shield 111-RB is a low slag, high deposition flux cored electrode designed for joining structural components made of low carbon steel. It is good over rust and primer.

Dual Shield 700X (70T-1)
Dual Shield 700X (70T-1)

Designed for flat and horizontal position welding using CO2 shielding gas, Dual Shield 700X provides high deposition rates, high efficiency and excellent performance.

Dual Shield 710X (71T-1/T-9)
Dual Shield 710X (71T-1/T-9)

Dual Shield 710X is an all-position flux cored wire that offers outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Dual Shield 710X-M
Dual Shield 710X-M

Dual Shield 710X-M is an all-position flux cored wire for general purpose welding.

Dual Shield ARC-87 (70T-1)
Dual Shield ARC-87 (70T-1)

Dual Shield Arc 87 is a low slag/high deposition efficiency flux cored wire designed for joining heavy structural components.

Dual Shield ARC-70 (70T-1/T-9)
Dual Shield ARC-70 (70T-1/T-9)

Dual Shield Arc 70 is a large diameter flux cored wire for flat and horizontal welding over heavy rust and mill scale.

Dual Shield R-70 Ultra (70T-1/T-9)
Dual Shield R-70 Ultra (70T-1/T-9)

Dual Shield R-70 Ultra is a low-fuming, high-deposition E70T-9 flux cored wire. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Dual Shield ARC-71 (71T-1)
Dual Shield ARC-71 (71T-1)

Dual Shield Arc 71 is a all-position welding over moderate rust and mill scale. Spatter levels and fume generation rates are lower than comparable cored wires.

Dual Shield 7000 (71T-1)
Dual Shield 7000 (71T-1)

Dual Shield 7000 is the industry's first all position flux cored wire combines excellent performance features with the ability to produce high quality welds.

Dual Shield 7100LC (71T-1/T-9)
Dual Shield 7100LC (71T-1/T-9)

Dual Shield 7100 LC is an all-position flux-cored wire for general purpose welding. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Dual Shield 7100 Ultra (71T-1/T-9)
Dual Shield 7100 Ultra (71T-1/T-9)

Dual Shield 7100 Ultra is an all-position E71T-9 flux-cored welding wire developed for higher deposition rates and improved welding productivity. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Dual Shield FC-717 (71T-1/T-9)
Dual Shield FC-717 (71T-1/T-9)

Dual Shield FC-717 is an all-position flux cored wire.

Dual Shield 70 Ultra Plus (71T-1/T-9)
Dual Shield 70 Ultra Plus (71T-1/T-9)

Dual Shield 70 Ultra Plus is an all-position wire that is uniquely designed to provide high deposition, outstanding all position performance and a fume emission rate approaching that of solid wires.

Dual Shield II 711X (71T-1/T-12)
Dual Shield II 711X (71T-1/T-12)

Dual Shield II 711X is an all-position flux cored wire that displays exceptional impact properties and toughness in combination with CO2 shielding gas.

Dual Shield II 71 Ultra (71T-1/T-12)
Dual Shield II 71 Ultra (71T-1/T-12)

Dual Shield II 71 Ultra is an all-position flux-cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.

Dual Shield II 70 Ultra (71 T-1/T-12)
Dual Shield II 70 Ultra (71 T-1/T-12)

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.

Dual Shield II 70T-12H4 (71T-1/T-12 )
Dual Shield II 70T-12H4 (71T-1/T-12 )

Dual Shield II 70T-12H4 is an all-position, low hydrogen flux cored wire that provides excellent low temperature toughness. This flux cored wire provides a smooth arc and low spatter levels, excellent for construction, fabrication, offshore and railcar applications.

Dual Shield II 712X (71T-1/T-12)
Dual Shield II 712X (71T-1/T-12)

Dual Shield II 712X is an all-position mixed gas flux cored wire intended for applications requiring outstanding weld metal toughness.

Dual Shield 110 (70T-2)
Dual Shield 110 (70T-2)

Dual Shield 110 has high deoxidation potential.

Dual Shield T-5 (71T-5)
Dual Shield T-5 (71T-5)

Dual Shield T-5 is a basic slag flux-cored wire that produces crack resistant, highly ductile weld deposits. It is especially produces recommended for medium to heavy fabrication, using a number of mild steels.

Dual Shield T-75 (70T-5/71T-5)
Dual Shield T-75 (70T-5/71T-5)

Dual Shield T-75 is a flux cored wire with a basic slag system designed for multiple pass welding and produces excellent properties in both the as welded and stress relieved conditions.