The Dual Shield line includes a broad range of formulations specifically developed for low alloy materials.
Dual Shield 7000-A1 is an all-position wire recommended for 0.5% Mo steels.
Dual Shield 8000-B2 is an all-position flux-cored wire containing 1% Cr - 0.5% Mo.
Dual Shield 8000-B2L is an all-position flux-cored wire for low carbon grades of 1. Cr - 0.5% Mo steels.
Dual Shield 88-CM is a flux cored continuous wire depositing X-ray sound weld metal with a nominal analysis of 1.25% Cr, 0.5% Mo.
Dual Shield 98-CM is a Cr-Mo flux-cored wire designed to weld 2% Cr - 1% Mo steels.
Dual Shield 9000-B3 is an all-position flux-cored wire containing 2% Cr-1% Mo.
Dual Shield 9000-B3L is an all-position flux cored wire for low carbon grades of 2.25% Cr - 1% Mo steels.
Dual Shield B6 is an all position flux cored wire designed to weld Mo steels.
Dual Shield B9 is an all position flux-cored wire designed to weld 9% Cr -1% Mo(P91) steels.
Dual Shield 88-C3 is a flux cored wire developed to deposit weld metal with impact toughness as low as -40ºF(-40ºC). The weld metal meets high X-ray standards for soundness.
Dual Shield II 80-Ni1H4 is an all position low-hydrogen welding wire that provides excellent low temperature toughness in both the as welded and/or stress relieved conditions when used with 75% Ar / 25% CO2. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.
Dual Shield 810X-Ni1 is an all position 1% Nickel flux cored wire for general purpose welding.
Dual Shield 8000-Ni2 is an all-position wire that deposits 2.5% Ni deposit with an 82 ksi (565 MPa) tensile strength.
Dual Shield 9000-C1 is an all-position flux-cored wire which produces a 2.5% Ni deposit.
Dual Shield II 100-D1 is an all-position flux cored welding wire specially formulated to weld quenched and tempered steels .
Dual Shield II 81-K2 is an all-position flux cored electrode developed for low alloy high strength steels where low temperature impact toughness is required. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.
Dual Shield II 90-K2 is an all-position, high performance wire with low diffusible hydrogen levels.
Dual Shield II 100 is an all-position wire that combines a high strength deposit with excellent impact toughness.
Dual Shield II 101H4M was developed to meet the stringent requirements of MIL-E-24403/2 and offshore welding, and it is an ideal choice for HSLA steels.
Dual Shield II 101-TC is an all-position wire developed to meet the U.S. Navy qualification tests for hydrogen levels of less than 0.05 ml/g of weld metal.
Dual Shield II 101-TM is an all-position flux cored wire developed to meet the stringent requirements of the military specification.
Dual Shield II 110 is an all-position flux cored wire which produces a smooth spray-like transfer, low spatter levels, easy slag removal and good arc direction.
Dual Shield II 120M2 is a high strength, low alloy flux cored wire for welding HY-100 and HSLA-100 steels.
Dual Shield T-95-M is a basic slag wire for HY-80 and other low alloy steels.
Dual Shield T-100 is a flux cored wire with excellent mechanical properties.
Dual Shield T-115 is a basic slag flux cored wire designed for applications requiring a high strength weld deposit.
Dual Shield 8100-W is an all-position wire for weathering grade steels.
Dual Shield T-4130 is a flux cored wire with a specialized weld metal analysis designed for welding alloy steels.
Dual Shield T-4130-LN is a basic slag flux cored electrode designed to match the heat treating properties of such steels as SAE 4130 and 8630 when the Nickel analysis of less than 1% is required.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.