Shield-Bright wires were specially developed for out-of-position welding and will deposit out-of-position welds at substantially higher welding currents than other stainless steel electrodes, for high deposition and maximum productivity. A self-peeling slag minimizes clean up.
Cryo-Shield 308L is an all-position stainless steel cored wire designed for low temperature cryogenic applications.
Shield-Bright 308L X-tra was developed to maximize performance in the flat and horizontal position on type 304 or 304L steels.
Shield-Bright 308L was developed for out-of-position welding on type 304 or 304L steels.
Shield-Bright 308H was developed for out-of-position welding on type 304H or 347H steels where high temperature service is required.
Shield-Bright 309LMo X-tra was developed to maximize performance in the flat and horizontal positions when joining or cladding stainless to low alloy steels.
Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.
Shield-Bright 309LMo was developed as an over-alloyed wire used in cladding and joining dissimilar metals.
Shield-Bright 309L was developed for out-of-position welding when joining stainless to mild or carbon steel.
Shield-Bright 309H was developed for out-of-position weld on 309H stainless where high temperature service is required.
Shield-Bright 312 was developed for out-of-position welding when joining stainless to high carbon and low alloy steels.
Shield-Bright 316L X-tra was developed to maximize performance in the flat and horizontal positions when improved corrosion resistance is needed on 316 and 316L steels.
Shield-Bright 316L was developed for out-of-position welding when improved corrosion resistance is needed on 316 and 316L steels.
Shield-Bright 316H was developed for out-of-position welding when required in high temperature service when using 316 steel.
Shield-Bright 317L X-tra was developed to maximize performance in the flat and horizontal position when the addition of molybdenum improves corrosion resistance.
Shield-Bright 317 was developed for out-of-position welding when the addition of Molybdenum improves corrosion resistance.
Shield-Bright 347H was developed for out-of-position welding when required in high temperature service on type 347.
Shield-Bright 347 was developed for out-of-position welding on types 347, 304, 304L, and 321 steels.
Shield-Bright 410NiMo was specifically designed for welding UNS S41500 wrought stainless steel CA-6NM (UNS J91540) cast steel and other similar 13Cr4NiMo steels commonly found on hydroelectric turbines and other similar applications.
Shield-Bright 2209 is a "duplex" stainless flux cored wire developed for out-of-position welding on 2209 or similar duplex steels.
Shield-Bright 2509 is a "super duplex" stainless flux cored wire developed for out-of-position welding on 2507 or similar super duplex steels.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.