Oxy-Fuel & MIG

All-State EASY GRIND
All-State EASY GRIND

Thie ideal wire for auto body repair or other light gauge applications. Welds over rust and paint when cleaning is not possible. Excellent match for today's high strength low alloy (HSLA) steel auto bodies. For the best results, use a 75% Argon/25% CO2 shielding gas mixture.

All-State E70S-6
All-State E70S-6

General purpose wire containing higher level of manganese and silicon.

All-State E70S-3
All-State E70S-3

General purpose wire.

All-State ER70S-2
All-State ER70S-2

Triple deoxidize wire.

All-State E70S-2
All-State E70S-2

Triple deoxidize wire.

All-State RG-65
All-State RG-65

A bare rod for braze welding of tubes, pipes, sheets, pressure vessels and tanks in the 65-75 ksi range. Provides higher weld strengths on low alloy steels.

All-State RG-60
All-State RG-60

A bare rod for braze welding on steel pipe, plates and structural shapes in 50-60 ksi range and castings.

All-State RG-45
All-State RG-45

A copper coated rod for braze welding on steel plate, sheet, pipe and wrought iron where strength up to 45 ksi required.