A general alloy for torch brazing and TIG welding or brazing of magnesium sheets, plates extrusions and castings. Argon or Argon/Helium gases is recommended when TIG welding.
A 50/50 lead/tin solder for sealing, joining or tinning most metals except aluminum. Not for food or medical use.
Special low temperature alloy used to restore and protect galvanized area of sheet and angle iron. Also use on cast iron for sealing, filling and repair cracks. Deposits are smooth and resist corrosion. Not for food or medical use.