All-State Aquasafe 100 Kit
All-State Aquasafe 100 Kit

Kit consists of 1 lb. (.45 kg) lead free cadmium free solder and 2 oz. tin of flux for joining copper and dissimilar metals in drinking water lines.

All-State Torchweld Powder Spray Kit
All-State Torchweld Powder Spray Kit

Joins and overlays cast iron, stainless steel & carbon steel. Torch can handle up to No. 90 single or multi-flame orifice tips.

All-State 430 DYNAGRIP KIT
All-State 430 DYNAGRIP KIT

Handy kit containing 4 ft. of 1/16" diameter All-State® No. 430 silver bearing solder and 1/2 fluid oz. of Duzall® flux.

All-State 509 STRONGSET KIT
All-State 509 STRONGSET KIT

Handy kit containing 4 ft. of 1/16" diameter solder and 1/2 fluid oz. of No. 509 flux.

All-State MAINTENANCE WELD KIT
All-State MAINTENANCE WELD KIT

Ten #1 plastic tubes of our most versatile TIG rods for Maintenance and Repair applications.