ESAB Submerged Arc fluxes are designed to deliver solutions for a variety of applications. A full line of fused and bonded fluxes are available to be used with a variety of carbon steel and stainless steel wires.
Bonded fluxes are made by dry mixing the ingredients, then bonding them together with a low melting point compound. Most bonded fluxes contain metallic deoxidizers that prevent weld porosity, especially important in fillet welds. Fine ingredients are mechanically bonded into larger particles for good performance with one mesh size.
Fused fluxes are made by mixing the ingredients, then melting them together to form a chemically homogenous product. Because the ingredients are completely reacted in the manufacture, you get smooth stable performance and consistent weld metal properties.
Stainless submerged arc fluxes can be used with solid and metal cored wires. Regardless of the application, Alloy Rods have the right flux for joining or cladding of stainless and duplex steels.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.