Fused fluxes are made by mixing the ingredients, then melting them together to form a chemically homogenous product. Because the ingredients are completely reacted in the manufacture, you get smooth stable performance and consistent weld metal properties.
OK Flux 50 is a neutral, fused flux that performs well in a wide variety of applications.
OK Flux 55 is a fused flux designed to make high speed butt and fillet welds in carbon steel sheet.