Print this page

Stainless Steel

Stainless Steel Submerged Arc Wires are manufactured under a carefully administered, high standard quality control program developed through years of experience in welding wire production. ESAB can supply these products as either solid or composite (metal cored) variations.

Alloy Shield 420 (No AWS Class)
Alloy Shield 420 (No AWS Class)

Alloy Shield 420 is a tubular, composite metal cored subarc wire designed for overlay shurfacing of steel mill rolls, picker rolls, crane wheels and similar applications where a hard surface is required. Can be used in combination with OK Flux 601.

Alloy Shield 410NiMo (EC410NiMo)
Alloy Shield 410NiMo (EC410NiMo)

Alloy Shield 410NiMo is a tubular, composite metal cored wire designed for welding CA-6NM castings or other similar Martensitic steels. Used in combination with 10.93 flux.

Alloy Shield 40S (No AWS Class)
Alloy Shield 40S (No AWS Class)

Alloy Shield 40S is a tubular, composite metal cored subarc wire designed for applications where metal-to-metal resistance is required. It produces nominally a 40-48 Rc hardness as welded when used in combination with 601 Flux after a 4 layer deposit.

Alloy Shield 30S (No AWS Class)
Alloy Shield 30S (No AWS Class)

Alloy Shield 30S is composite metal cored subarc wire designed to be used for build-up and for hardfacing applications where moderate hardness and good machinability are important. Designed to be used with 601 Flux.

Arcaloy ER308L (ER308/308L)
Arcaloy ER308L (ER308/308L)

Arcaloy ER308L is a low carbon grade of 308 designed for MIG or TIG of stainless steels such as AISI 301, 304, 304L steels.

Arcaloy ER308/308H (ER308/308H)
Arcaloy ER308/308H (ER308/308H)

Arcaloy ER308/308H is a high carbon grade of 308 for higher temperature requirements. Can be used in combination with OK Flux 10.93 or 10.95.

Arcaloy ER309L (ER309/309L)
Arcaloy ER309L (ER309/309L)

Arcaloy ER309L is a continuous, solid, corrosion-resisting chromium-nickel wire for joining stainless steels to non-alloy or low alloy steels as well as welding of austenitic stainless alloys of 24% Cr, 13% Ni types. Arcaloy ER309L can be used in combination with OK Flux 10.93 or 10.94.

Arcaloy ER316L (ER316/316L)
Arcaloy ER316L (ER316/316L)

Arcaloy ER316L is a continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding austenitic stainless alloys of he 18% Cr, 8% Ni, and 18 % Cr, 8% Ni, 3% Mo types. Arcaloy ER316L can be used in combination with OK Flux 10.93 or 10.94.

Arcaloy ER317L (ER317/317L)
Arcaloy ER317L (ER317/317L)

Arcaloy 317L is a continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding of austenitic stainless alloys of 19% Cr, 13% Ni, 3% Mo types.

OK Autrod 308L (ER308L)
OK Autrod 308L (ER308L)

OK Autrod 308L is a low carbon MIG wire and has good general corrosion resistance.

OK Autrod 309L (ER309L)
OK Autrod 309L (ER309L)

OK Autrod 309L is a continuous, solid, corrosion-resisting chromium-nickel wire for joining stainless steels to non-alloy or low alloy steels as well as welding of austenitic stainless alloys of 24% Cr, 13% Ni types. OK Autrod 309L can be used in combination with OK Flux 10.93 or 10.94.

OK Autrod 316L (ER316L)
OK Autrod 316L (ER316L)

OK Autrod 316L is a continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding austenitic stainless alloys of he 18% Cr, 8% Ni, and 18 % Cr, 8% Ni, 3% Mo types. OK Autrod can be used in combination with OK Flux 10.93 or 10.94.

OK Autrod 2209 (ER2209)
OK Autrod 2209 (ER2209)

OK Autrod 2209 (16.86) is a continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo type. OK Autrod 2209 can be used in combination with OK Flux 10.93.

OK Autrod 2509 (No AWS Class)
OK Autrod 2509 (No AWS Class)

OK Autrod 2509 is continuous, solid, corrosion-resistant, "Super Duplex" wire for welding austenitic-ferritic stainless alloys of the 25% Cr, 10% Ni, 4% Mo, low Carbon type. Ok Autrod 2509 can be used in combination with OK Flux 10.94

OK Autrod 12.24
OK Autrod 12.24

ESAB Welding & Cutting Products introduces OK Autrod 12.24, a molybdenum- alloyed, copper-coated wire for submerged arc welding of non-alloyed and low-alloyed steels.

OK Band 308L (EQ308L)
OK Band 308L (EQ308L)

OK Band 308L is a stainless welding strip designed for cladding using the submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 308L produces a 308L deposit.

OK Band 309L (EQ309L)
OK Band 309L (EQ309L)

OK Band 309L is a stainless strip for cladding using the (SAW)submerged arc welding process. Band 309L and OK Flux 10.05 provides a buffer layer when used with 308L, 316L, 317L, or 347 to produce the desired analysis on the second layer.

OK Band 309LMo (EQ309LMo)
OK Band 309LMo (EQ309LMo)

OK Band 309LMo is a stainless strip for single layer electroslag strip cladding. OK Band 309LMo together with OK Flux 10.10, produces a 316L weld deposit analysis in one layer.

OK Band 309LNb (EQ309LNb)
OK Band 309LNb (EQ309LNb)

OK Band 309LNb is a stainless strip for single layer electroslag strip surfacing. Band 309LNb together with OK Flux 10.10 produces a 347 weld deposit analysis in one layer.

OK Band 316L (EQ316L)
OK Band 316L (EQ316L)

OK Band 316L is a stainless welding strip for designed for cladding using submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 316L produces a 316L deposit.

OK Band 347 (EQ347)
OK Band 347 (EQ347)

OK Band 347 is a stainless welding strip designed for cladding using submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 347 produces a 347 deposit.