Nickel

ESAB nickel-based alloys are specially formulated and designed to meet a variety of corrosion resistant and low temperature cryogenic applications. Coupled with one of the many fluxes, it produces excellent mechanical properties that confirm to various approvals and customer specifications.

Arcaloy ER625
Arcaloy ER625

Arcaloy ER625 is a Ni-Cr-Mo alloy designed for cladding iron and joining similar steels or dissimilar steels such as stainless and low alloy materials.

Arcaloy ER276
Arcaloy ER276

Arcaloy ER276 is a Ni-Cr-Mo alloy designed for joining or cladding where resistance to stress corrosion cracking, pitting and crevice corrosion is essential.