All Arcaloy and Autrod products have been designed and developed around a "matte" surface finish that provides for more trouble-free welding. These wires' columnar strength allows for higher wire feed speed and greater productivity. Our control on wire cast and helix minimizes downtime while providing better welding performance. Choose from one of our many alloys and see the difference.

OK Autrod 16.95 (307Si, No AWS Class)
OK Autrod 16.95 (307Si, No AWS Class)

OK Autrod 16.95 (307Si) is a high silicon MIG wire that improves wetting characteristics of the weld deposit. This alloy is used for joining of austenitic, manganese, work-hardenable steels, as well as armour plate and heat-resistant steels.

Arcaloy ER308L (ER308/308L)
Arcaloy ER308L (ER308/308L)

Arcaloy ER308L is a low carbon grade of 308 designed for MIG or TIG of stainless steels such as AISI 301, 304, 304L steels. SPECIAL ORDER ONLY

Arcaloy ER308/308H (ER308/308H)
Arcaloy ER308/308H (ER308/308H)

Arcaloy ER308/308H has good corrosion resistance in high temperature service.

ESAB ER308LSi MIG (ER308Si/308LSi)
ESAB ER308LSi MIG (ER308Si/308LSi)

ESAB ER308LSi MIG is a silicon enhanced MIG wire which significantly increases wetting action, resulting in a smooth weld to improve weldability and performance on 304 steels.

Arcaloy ER309L (ER309/309L)
Arcaloy ER309L (ER309/309L)

Arcaloy ER309L is a low carbon grade of 309 for MIG or TIG welding.

ESAB ER309LSi MIG (ER309Si/309LSi)
ESAB ER309LSi MIG (ER309Si/309LSi)

ESAB ER309LSi MIG is a silicon enhanced grade of 309 which improves the welding properties such as wetting. It has good general corrosion resistance.

Arcaloy ER310 (ER310)
Arcaloy ER310 (ER310)

Arcaloy ER310 is used to weld stainless steel of similar composition.

Arcaloy ER316L (ER316/316L)
Arcaloy ER316L (ER316/316L)

Arcaloy ER316L is a low carbon grade of stainless steel which provides additional corrosion resistance where necessary.

ESAB ER316LSi MIG (ER316Si/316LSi)
ESAB ER316LSi MIG (ER316Si/316LSi)

ESAB ER316LSi MIG is a low carbon, high silicon grade of 316. The addition of silicon improves the weldability and performance.

Arcaloy ER347 (ER347)
Arcaloy ER347 (ER347)

Arcaloy ER347 is a columbium stabilized stainless steel for welding types 347 and 321 stainless, comes in MIG, TIG, and SAW forms.

Arcaloy ER409Nb (ER409Nb)
Arcaloy ER409Nb (ER409Nb)

Arcaloy ER409Nb is a ferritic stainless steel stabilized with Niobium for joining 409 stainless.

OK Autrod 2209 (ER2209)
OK Autrod 2209 (ER2209)

OK Autrod 2209 is a duplex stainless steel for welding type 2205 duplex stainless.