All GTAW nickel based products are similarly produced (as are the ESAB stainless MIG wire), and meet a variety of demanding specifications. The chemically-cleaned wire surface prevents unnecessary impurities frequently associated with other TIG rods. All rods are marked with the proper identification to avoid lot mixups. The various grades and alloys make ESAB TIG products the first choice of welders.
Arcaloy ER276 is a Ni-Cr-Mo alloy designed for joining or cladding where resistance to stress corrosion cracking, pitting and crevice corrosion is essential.
Arcaloy ER82 is used for TIG, MIG, and SAW welding of base materials such as ASTM B163, B166, B167, and B168 alloys which have UNS Number N0660.
Arcaloy ERNiCu-7, commonly referred to as Alloy FM60 is a GTAW (gas tungsten arc welding) product for welding nickel copper alloys such as ASTM B127, B163, B164 & B165, UNS number N04400.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.