Purox® W-300 Welding Torch

W-300 Welding Torch

Features

  • Ideal for all welding, brazing or medium heating applications in average production, repair or maintenance work.
  • Recommended for manual operations requiring speed and uninterrupted welding, heating and brazing.
  • Operates on medium pressure acetylene and other fuel gases.
  • Gas-mixer – high resistance to backfires, flame pops and flashbacks.
  • Roll stamped permanent identification.
  • Extra length Teflon valve packing for improved backlash characteristics.

Classifications

Specifications

Purox W-300 Welding Torch
Welding Torches  
Welding Range Thin Gauge to over 1 in.
Heating Range 1 to 200 cfh acetylene, 1400 to 300,000 Btu/hr.
Capacity  
Acetylene Flow 200 CFH
Max. Welding 1 in.
Consumables  
Welding Heads W-300
Physical  
Net Weight 1.3 lbs.
Length 7-3/4 in.
Hoses Conn. B

Ordering