Oxygen-Fuel Gas Shutoff Valve V-27

The V-27 shutoff valve is used in flame-hardening, machine cutting, etc., for quick-acting on/off control of oxygen and fuel gas with a single lever.

Features

  • The V-27 Valve is supplied with appropriate 1/4 in. NPT to "B" size inlet and outlet connection fittings, packed loose.
V-27

Classifications

Specifications

V-27
Maximum Operating Pressures and Specifications  
Oxygen 150 PSIG, 1035 kPa
Acetylene 15 PSIG, 103 kPa
Other Fuel Gases 75 PSIG, 517 kPa
Height 6-3/4 in, 172 mm
Width 3-5/8 in, 92 mm
Length 5-1/2 in, 140 mm

Ordering

Configure this Model

Part No.

V-27
Part No. Model / Product Description UPC
20X25 VALVE V27 SHTF QAC DB 662067029945

Accessories

There are no accessories.

Package Contents

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.