High speed with low acetylene consumption. Divergent Bore Cutting Oxygen Hole.

| Metal Thickness | 1/2-14 in., 13-350 mm |
|---|---|
| Nozzle Size | 1/2-14 |
| No. Preheat Holes or Slots | 6 or 8 |
| Gas Pressure | |
| Cutting Oxygen | 90-120 PSIG |
| Preheat Oxygen | 20-65 PSIG |
| Cutting Acetylene | 5-13 PSIG |
| Cutting Speed | 3-30 ipm |
| Gas Consumption | |
| Total Oxygen | 60-1525 CFH |
| Acetylene | 5-51 CFH |
| Average Kerf Width | .052-.240 in. |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 639171 | 1563 NOZZLE 1/2 IN | 662067016655 |
| 639172 | 1563 NOZZLE 3/4 IN | 662067016662 |
| 639173 | 1563 NOZZLE 1 IN | 662067016679 |
| 639174 | 1563 NOZZLE 11/2 IN | 662067016686 |
| 639175 | 1563 HS NOZZLE 2 IN | 662067016693 |
| 639176 | 1563 NOZZLE 21/2 IN | 662067016709 |
| 639177 | 1563 NOZZLE 4 IN | 662067016716 |
| 639178 | 1563 NOZZLE 6 IN | 662067016723 |
| 998747 | 1563 NOZZLE #10 | 662067016747 |
| 998748 | 1563 NOZZLE #14 UTD | 662067016754 |
| 639179 | 1563 NOZZLE 8 IN | 662067016730 |
| There are no accessories. |
|---|
***Do not use with low pressure acetylene. *Use where high preheat intensity is desired.
To clean preheat slots, remove external sleeve and use a soft bristled brush.
NOTE – DO NOT clean with notched-type wires or twist drills since any metal removal from the passages will destroy the precision cutting characteristics. Use the non-cutting wires and taper reamers included in OXWELD® Cleaning Kit (Part No. 755F00). For longer life, nozzles should be cleaned periodically
in a solution of OXWELD® nozzle cleaning compound (Part No. 761F00). The cutting orifice of these nozzles should be cleaned only with OXWELD® nozzle cleaning compound.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.