Oxweld W-500 Rosebud Style Multiflame Heating Heads

Oxweld W-500 Rosebud Style Multiflame Heating Heads

Features

Classifications

Specifications

Oxweld W-500 Rosebud Style Multiflame Heating Heads
Rosebud Style Multiflame Heating Heads  
For Oxy-Acetylene Use  
Head Size 70 - 250 O - A
No. of Flames 9 - 16
Average Heat Output 103,000 - 368,000 Btu/hr.
For Oxy-Fuel Gas Use  
Head Size 200/500 O - FG
No. of Flames 24/29
Average Heat Output 500,000 - 1.2m Btu/hr.

Ordering

Configure this Model

Part No.

Oxweld W-500 Rosebud Style Multiflame Heating Heads
Part No. Model / Product Description UPC
998834 W-500 #70 0-A ROSEBUD 662067021819
998835 W-500 #100 0-A ROSEBUD 662067021826
998836 W-500 #200 0-A ROSEBUD 662067021833
998837 W-500 #250 0-A ROSEBUD 662067021840
999236 W-500 #200 0-FG ROSEBUD 662067021864
999088 W-500 #500 0-FG ROSEBUD 662067021888