Oxweld Hydraulic Fuel Gas Protective Devices H-18/H-19

Oxweld Hydraulic Fuel Gas Protective Devices H-18/H-19 have flashback and backflow protection to satisfy OSHA Regulations.

Features

  • Rated fuel gas capacities to 23,000 cfh @ 100 psig
  • Meets OSHA requirements and NFPA Standards/UL Listed
  • Heavy-duty welded steel shell construction
  • Models for all fuel gases
  • Flashback and backflow protection to satisfy OSHA Regulations
  • Contains relief valve

Classifications

Specifications

Oxweld H-18/H-19
Protective Devices  
Hydraulic Protective Devices  
Fuel Gas Flow Capacities for Inlet Pressures Other than 15 PSIG  
Capacity  
H-18 600-3900
H-19 1800-11,500
Maximum Inlet Pressure  
H-18 20 or 100 PSIG
H-19 20 or 125 PSIG
Rated Flow @ 15 PSI  
H-18 1000 CHF
H-19 3000 CHF
Height  
H-18 19 in.
H-19 38 in.
Pot. Max. Dia.  
H-18 13 in.
H-19 13 in.
Inlet & Outlet Connections  
H-18 1-1/4 in. NPTF
H-19 2 in. NPTF
Relief Valve Conn.  
H-18 3/4 in. NPTF
H-19 3/4 in. NPTF
Shipping Weight  
H-18 150 lbs.
H-19 180 lbs.

Ordering

Configure this Model

Part No.

Oxweld H-18/H-19
Part No. Model / Product Description UPC
09P68 HYD BCK PRESS VLV H-18 FG 100P  
09P69 HYD BCK PRESS VLV H-19 FG 125P 662067075829
11P99 HYD BACK PRES VLV H-19 FG 20PS 662067076970
12P02 HYD BCK PRESS VLV H-18 FG 100P 662067077137

Accessories

There are no accessories.

Package Contents

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.