OXWELD® AC-4 Powder Cutting Hand Torches

Features

  • Rapidly cut any thickness stainless steel, cast iron and high alloy steels
  • As simple to use as regular cutting torches
  • Manual or mechanized versions available
  • Self Contained
  • Capacity 10 in. thick stainless
  • Acetylene or fuel gas
  • Single lever control

Classifications

Specifications

OXWELD AC-4 Torch
Powder Cutting Equipment  
Length 28 or 44 in
Head Angle 75 or 180 deg.
Ship Weight 22 or 30 lbs
Inlet Connections 3/8 in. - "B" size

Ordering

Configure this Model

Part No.

OXWELD AC-4 Torch
Part No. Model / Product Description UPC
02X60 AC-4-28-75 POWDER TORCH 662067075294
2117245 AC-4-44-180 POWDER TORCH 662067091447
220234 AC-4-28-180 POWDER TORCH 662067094806
28X65 AC-4-44-75 POWDER TORCH 662067109647

Accessories

There are no accessories.

Package Contents

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.