Oxweld W-500 Acetylene Welding Heads

W-500 Acetylene Welding Heads (Single Flame)

Ordering Information
SKU20336
UPC662067018352
Model / Product DescriptionW-500 #30 WLD HEAD
Item Weight0.00
Min Order 
Acetylene Welding/Heating Heads (Single Flame) 
Steel Thickness3/16-3/8 in
Head Size30A
C Flame Tips 
Brazes0 to 0 in