Oxweld W-500 Acetylene Welding Heads

W-500 Acetylene Welding Heads (Single Flame)

Ordering Information
SKU998116
UPC662067018475
Model / Product DescriptionW-500 #70 WLDG HD
Item Weight0.00
Min Order 
Acetylene Welding/Heating Heads (Single Flame) 
Steel Thickness5/8-1 in
Head Size70A
C Flame Tips 
Brazes to in