These Swirljet tips are designed to be used with the PREST-O-LITE® #1 Quick Disconnect torch handle. They run quieter and cooler and give better heat transfer than other comparable tips.
| SKU | 22593 |
|---|---|
| UPC | 662067997763 |
| Model / Product Description | SWIRLJET AY QD SJ-2A |
| Item Weight | 0.00 |
| Min Order | |
| Acetylene Swirljet Tips | |
| Fuel | Acetylene |
| Pressure | 13 PSIG |
| Gas Flow | 5.7 CFH |
| Copper Tubing Size And Capacity | |
| Soft Solder | 3/4-1-1/2 in |
| Silver Braze | 1/4-3/4 in |