Print this page

Plasmarc™ PT-27 Torch

Designed for superior cutting performance and ease of handling, the PT-27 produces clean, exceptionally high quality cuts.

Features

  • Most compact 80 amp torch on the market
  • Excellent cutting capacity—cuts up to 1 in. (25.4 mm); severs up to 1-1/4 in. (31.75 mm)
  • Uses shop air, cylinder air or nitrogen for superior versatility
  • Pilot arc starting—even starts through paint
  • Choice of 25 ft. (7.6 m) or 50 ft. (15.2 m) line length
  • Perfect electrode centering
  • Intermittent cutting capability for grate or expanded metal applications
  • Use with three cutting nozzle sizes for exceptional versatility
  • Improved spring-loaded seat eliminates head burn-out
  • One-year warranty

Classifications

Specifications

PT-27
Cuts 1.0 in, 25.4 mm
Severs 1-1/4 in, 31.75 mm
Current Capacity  
100% Duty Cycle 80 Amps
Air Supply 65 to 75 PSIG, 320 CFH, 150 l/min, 5.2 to 5.5 bars
Length of Service Lines 25 ft, 7.6 m, 50 ft, 15.2 m
Dimensions  
Overall Length 7.3 in, 185 mm
Length of Head 3.06 in, 78 mm

Ordering Information

Configure this Model

Part No.

PT-27
Part No. Model / Product Description UPC
Q21616 PT-27 HEAT SHIELD 662067168606
Q33366 PT-27 ELECTRODE (2) 662067163557
Q33367 PT-27 BAFFLE 662067168040
Q33368 PT-27 30 AMP NOZZLE (5)  
Q33369 PT-27 50-70 AMP NOZZLE (5) 662067163564
Q33418 PT-27 80 AMP NOZZLE (5) 662067168125
821620 TORCH AY PT-27 75 25' ARC PLUG  
821621 TORCH AY PT-27 75 50' ARC PLUG  
835548 PT-27 75 25' ARC RING & LHS  
835764 PT 27 75 DEG 50 LHS TOR W/PLG  
821623 KIT SP PTS PT 27 50-70 AMP  
821624 KIT SP PTS PT 27 80 AMP  
835776 KIT S/P PT-27 LHS 50-70 AMP  
821420 GUIDE STAND-OFF PT-23, PT-27  
821616 *PT-27 HEAT SHIELD  
835547 SHIELD HEAT LONG PT-27  
0558003030 VALVE PIN SHELL PT-27  
0558003031 ELECTRODE SEAT PT-27  
80558003032 SEAT AY PT-27  
35548 PT-27 75 25' ARC RING & LHS 662067022298
21621 TORCH AY PT-27 75 50' ARC PLUG 662067038084
21620 TORCH AY PT-27 75 25' ARC PLUG 662067038077
21661 TORCH AY PT-27 75 25' ARC RING 662067021895
21662 TORCH AY PT-27 75 50' ARC RING 662067022052

Accessories

There are no accessories.

Cut Speed

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.