Shield-Bright 308H was developed for out-of-position welding on type 304H or 347H steels where high temperature service is required.
Shield-Bright 308L was developed for out-of-position welding on type 304 or 304L steels.
Shield-Bright 308L X-tra was developed to maximize performance in the flat and horizontal position on type 304 or 304L steels.
Shield-Bright 309L was developed for out-of-position welding when joining stainless to mild or carbon steel.
Shield-Bright 309LMo was developed as an over-alloyed wire used in cladding and joining dissimilar metals.
Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.
Shield-Bright 309LMo X-tra was developed to maximize performance in the flat and horizontal positions when joining or cladding stainless to low alloy steels.
Shield-Bright 312 was developed for out-of-position welding when joining stainless to high carbon and low alloy steels.
Shield-Bright 316H was developed for out-of-position welding when required in high temperature service when using 316 steel.
Shield-Bright 316L was developed for out-of-position welding when improved corrosion resistance is needed on 316 and 316L steels.
Shield-Bright 316L X-tra was developed to maximize performance in the flat and horizontal positions when improved corrosion resistance is needed on 316 and 316L steels.
Shield-Bright 317 was developed for out-of-position welding when the addition of Molybdenum improves corrosion resistance.
Shield-Bright 347 was developed for out-of-position welding on types 347, 304, 304L, and 321 steels.
Shield-Bright 347H was developed for out-of-position welding when required in high temperature service on type 347.
Shield-Bright 2209 is a "duplex" stainless flux cored wire developed for out-of-position welding on 2209 or similar duplex steels.
Shield-Bright 2594 is a "super duplex" stainless flux cored wire developed for out-of-position welding on 2507 or similar super duplex steels.