Print this page

SHIELD-BRIGHT 308L

Shield-Bright 308L was developed for out-of-position welding on type 304 or 304L steels.

Features

Shield-Bright 308L was developed for welding type 304L stainless steel and can also be used for welding types 301, 302, and 304 steels. It may also be used for welding types 321 and 347 if the service conditions do not exceed an approximate of 750°F (399°C).

Shield-Bright 308L was designed for welding in all position and performs particularly well in the vertical position with excellent slag removal.

* This item is subject to Industry Alloy Surcharges

Shield-Bright 308L
  • Industry
  • Mobile Machinery
  • General Fabrication
  • Shipbuilding
  • Process
  • Pipeline
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 6
    • MIL-STD-1689 APPLICATIONS-NAVY
    • ASME II SFA 5.22; E308LT1-1/T1-4
    • TUV
    • CERTIFIED by CWB - AWS A5.22
    • ABS - AWS A5.22; E308LT1-1

Properties

Typical Properties
As Welded using 75% Ar - 25% CO2  
Tensile Strength 85 ksi, 580 MPa
Yield Strength 60 ksi, 410 MPa
Elongation in 2" 44 %
Typical Undiluted Weld Metal Analysis  
100% CO2  
C 0.03%
Mn 1.2%
Si 0.8%
Cr 19%
Ni 10%
Mo 0.1%
Cu 0.15%
Ferrite 7 FN
75% Ar / 25% CO2  
C 0.03%
Mn 1.2%
Si 0.9%
Cr 19%
Ni 10%
Mo 0.1%
Cu 0.15%
Ferrite 7 FN

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100 A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100% CO2