Shield-Bright 308L X-tra was developed to maximize performance in the flat and horizontal position on type 304 or 304L steels.
Shield-Bright 308L X-tra was designed for welding type 304L stainless steel but can be used for types 301, 302,and 304 steels. It may also be used successfully for welding of types 321 and 347 stainless steel. Service conditions should not exceed an approximate of 750°F (399°C).
Shield-Bright 308L X-tra was designed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.
* This item is subject to Industry Alloy Surcharges

| As Welded using 75% Ar - 25% CO2 | |
|---|---|
| Tensile Strength | 85 ksi, 580 MPa |
| Yield Strength | 60 ksi, 410 MPa |
| Elongation in 2" | 40 % |
| Typical Undiluted Weld Metal Analysis | |
| 100% CO2 | |
| C | 0.025% |
| Mn | 1.3% |
| Si | 0.9% |
| Cr | 19.5% |
| Ni | 9.8% |
| Mo | 0.1% |
| Cu | 0.15% |
| Ferrite | 8 FN |
| 75% Ar / 25% CO2 | |
| C | 0.022% |
| Mn | 1.4% |
| Si | 0.9% |
| Cr | 19.6% |
| Ni | 9.9% |
| Mo | 0.1% |
| Cu | 0.15% |
| Ferrite | 8 FN |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 150 A | 25 | 259 ipm, 6.6 cm/min | 5 lbs./hr., 2.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 200 A | 29 | 410 ipm, 10.4 cm/min | 7.7 lbs./hr., 3.5 kg./hr. | 84.2 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 33 | 860 ipm, 21.9 cm/min | 16.9 lbs./hr., 7.7 kg./hr. | 87 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 200 A | 25 | 172 ipm, 4.4 cm/min | 6.7 lbs./hr., 3.1 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 240 A | 28 | 225 ipm, 5.7 cm/min | 8.1 lbs./hr., 3.7 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 400 A | 33 | 495 ipm, 12.58 cm/min | 18.9 lbs./hr., 8.6 kg./hr. | 85.5 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2 or 100% CO2