SHIELD-BRIGHT 309LMo

Shield-Bright 309LMo was developed as an over-alloyed wire used in cladding and joining dissimilar metals.

Features

Shield-Bright 309LMo was designed for welding type 316 clad steels on the first pass in cladding steels or for welding dissimilar metals such as molybdenum-containing austenitic stainless steels to carbon steels. It is used in paper mills and in power plants to give greater corrosion resistance. This wire performs best when used out-of-position shielded with either Argon/CO2 or 100%CO2.

* This item is subject to Industry Alloy Surcharges

Shield-Bright 309LMo
  • Industry
  • General Fabrication
  • Pulp and Paper
  • Process
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 6
    • AWS A5.22; E309LMoT1-1/T1-4
    • ASME II SFA 5.22; E309LMoT1-1/T1-4

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Tensile Strength 90 ksi, 620 MPa
Yield Strength 70 ksi, 480 MPa
Elongation in 2" 30 %
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.03 %
Mn 1.0 %
Si 0.6 %
Cr 23 %
Ni 13.5 %
Mo 2.5 %
Cu 0.1 %
Ferrite 19 FN
As Welded 75% Ar / 25% CO2  
C 0.03 %
Mn 1.2 %
Si 0.75 %
Cr 23.5 %
Ni 13.5 %
Mo 2.5 %
Cu 0.1 %
Ferrite 21 FN

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100A A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75% Ar / 25% CO2 or 100% CO2