Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.
Shield-Bright 309L X-tra was developed for the welding of stainless steels to carbon or low alloy steels and for the first layer cladding of carbon and low alloy steels. Shield-Bright 309L X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.
For joining thick sections, it is preferred the non-stainless steel be buttered with a layer of Shield-Bright 309L X-tra and the joint completed with Shield-Bright 316L X-tra or 308L X-tra. The service temperature should not exceed approximately 750ºF (399ºC).
* This item is subject to Industry Alloy Surcharges

| As Welded 75% Ar / 25% CO2 | |
|---|---|
| Tensile Strength | 87 ksi, 600 MPa |
| Yield Strength | 70 ksi, 480 MPa |
| Elongation in 2" | 35 % |
| Typical Undiluted Weld Metal Analysis | |
| As Welded CO2 | |
| C | 0.03 % |
| Mn | 1.3 % |
| Si | 0.7 % |
| Cr | 24 % |
| Ni | 12.5 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Ferrite | 16 FN |
| As Welded 75% Ar / 25% CO2 | |
| C | 0.03 % |
| Mn | 1.4 % |
| Si | 0.8 % |
| Cr | 24.5 % |
| Ni | 12.5 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Ferrite | 18 FN |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 150 A | 25 | 259 ipm, 6.6 cm/min | 5 lbs./hr., 2.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 200 A | 29 | 410 ipm, 10.4 cm/min | 7.7 lbs./hr., 3.5 kg./hr. | 84.2 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 33 | 860 ipm, 21.9 cm/min | 16.9 lbs./hr., 7.7 kg./hr. | 87 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 200 A | 25 | 172 ipm, 4.4 cm/min | 6.7 lbs./hr., 3.1 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 240 A | 28 | 225 ipm, 5.7 cm/min | 8.1 lbs./hr., 3.7 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 400 A | 33 | 495 ipm, 12.58 cm/min | 18.9 lbs./hr., 8.6 kg./hr. | 85.5 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2 or 100%CO2