Shield-Bright 316L was developed for out-of-position welding when improved corrosion resistance is needed on 316 and 316L steels.
Shield-Bright 316L was developed for the welding of Type 316L stainless steel but can be used for other stainless steels including Types 316 and 304L. In a few cases, e.g. nitric acid service, Shield-Bright 316L should not be used to weld 304L. It contains molybdenum which resists pitting corrosion induced by sulphuric and sulphurous acids, chlorides and cellulose solutions. Used widely in the rayon, dye and paper making industries.
Shield-Bright 316L was developed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.

| As Welded 75% Ar / 25% CO2 | |
|---|---|
| Tensile Strength | 85 ksi, 580 MPa |
| Yield Strength | 65 ksi, 450 MPa |
| Elongation in 2" | 40 % |
| Typical Undiluted Weld Metal Analysis | |
| As Welded CO2 | |
| C | 0.03 % |
| Mn | 1.2 % |
| Si | 0.8 % |
| Cr | 18.5 % |
| Ni | 12 % |
| Mo | 2.7 % |
| Cu | 0.15 % |
| Ferrite | 8 FN |
| As Welded 75% Ar / 25% CO2 | |
| C | 0.03 % |
| Mn | 1.2 % |
| Si | 0.9 % |
| Cr | 18.5 % |
| Ni | 12 % |
| Mo | 2.7 % |
| Cu | 0.15 % |
| Ferrite | 8 FN |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 100 A | 23 | 265 ipm, 6.7 cm/min | 2.9 lbs./hr., 1.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 130 A | 25 | 227 ipm, 5.8 cm/min | 4.25 lbs./hr., 1.9 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 165 A | 26 | 341 ipm, 8.7 cm/min | 6.14 lbs./hr., 2.8 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 190 A | 28 | 445 ipm, 11.3 cm/min | 8.08 lbs./hr., 3.7 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 220 A | 30 | 567 ipm, 14.4 cm/min | 10.24 lbs./hr., 4.6 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 170 A | 25 | 154 ipm, 3.9 cm/min | 5.34 lbs./hr., 2.4 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 210 A | 27 | 193 ipm, 4.9 cm/min | 6.89 lbs./hr., 3.1 kg./hr. | 82.5 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 250 A | 28 | 243 ipm, 6.2 cm/min | 8.57 lbs./hr., 3.9 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 29 | 321 ipm, 8.2 cm/min | 11.43 lbs./hr., 5.2 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2 or 100%CO2