Shield-Bright 316L X-tra was developed to maximize performance in the flat and horizontal positions when improved corrosion resistance is needed on 316 and 316L steels.
Shield-Bright 316L X-tra was developed for the welding Type 316L stainless steel and also can be used for the other stainless steels including Types 316 and 304L. In a few cases, e.g. nitric acid service, Shield-Bright 316L X-tra should not be used to weld 304L. It was designed specifically for applications where the service environment can produce pitting corrosion.
Shield-Bright 316L X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.
* This item is subject to Industry Alloy Surcharges

| As Welded using 75% Ar - 25% CO2 | |
|---|---|
| Tensile Strength | 65 ksi, 450 MPa |
| Yield Strength | 85 ksi, 580 MPa |
| Elongation in 2" | 36 % |
| Typical Undiluted Weld Metal Analysis | |
| 100% CO2 | |
| C | 0.03% |
| Mn | 1.2% |
| Si | 0.6% |
| Cr | 18.5% |
| Ni | 12% |
| Mo | 2.7% |
| Cu | 0.15% |
| Ferrite | 7 FN |
| 75% Ar / 25% CO2 | |
| C | 0.03% |
| Mn | 1.3% |
| Si | 0.6% |
| Cr | 19% |
| Ni | 12% |
| Mo | 2.7% |
| Cu | 0.15% |
| Ferrite | 8 FN |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 150 A | 25 | 259 ipm, 6.6 cm/min | 5 lbs./hr., 2.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 200 A | 29 | 410 ipm, 10.4 cm/min | 7.7 lbs./hr., 3.5 kg./hr. | 84.2 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 33 | 860 ipm, 21.9 cm/min | 16.9 lbs./hr., 7.7 kg./hr. | 87 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 200 A | 25 | 172 ipm, 4.4 cm/min | 6.7 lbs./hr., 3.1 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 400 A | 33 | 495 ipm, 12.58 cm/min | 18.9 lbs./hr., 8.6 kg./hr. | 85.5 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2 or 100%CO2