Print this page

SHIELD-BRIGHT 2209

Shield-Bright 2209 is a "duplex" stainless flux cored wire developed for out-of-position welding on 2209 or similar duplex steels.

Features

Shield-Bright 2209 was developed for the welding of '2205' duplex stainless steels e.g. UNS S31803, S32205, and J92205. It can also be used for the welding of leaner grades of duplex stainless steels. It has been approved with a 25ºC critical pitting temperature and impact toughness at -40ºF (-40ºC). Shield-Bright 2209 was developed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.

* This item is subject to Industry Alloy Surcharges

Shield-Bright 2209
  • Industry
  • Petrochemical
  • Pulp and Paper
  • Process
  • Pipeline
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.22; E2209T1-4
    • ASME II SFA 5.22 E2209T1-4
    • ABS
    • ASME IX F No. 6
    • D.N.V.- For Duplex S/S
    • L.R.- S 31803 S
    • A.B.S.- AWS A5.22; E2209T1-4
    • TUV

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Stress 95 ksi, 650 MPa
Tensile Strength 120 ksi, 820 MPa
Elongation in 2" 25 %
V-Notch Impact Toughness  
Absorbed Energy @ -4ºF (-20ºC) 45 ft.-lbs., 61 J
Absorbed Energy @ -40ºF (-40ºC) 40 ft.-lbs., 54 J
Absorbed Energy @ -60ºF (-51ºC) 35 ft.-lbs., 47 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.03 %
Mn 0.9 %
Si 0.35 %
Cr 22.5 %
Ni 9.2 %
Mo 3 %
Cu 0.1 %
N 0.16 %
Ferrite 35 FN

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100A A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2