Shield-Bright 2509 is a "super duplex" stainless flux cored wire developed for out-of-position welding on 2507 or similar super duplex steels.
Shield-Bright 2509, a "super duplex" stainless cored wire, was developed with a nominal composition of 25% Cr, 9% Ni, 4% Mo, and 0.25% N. This cored wire is manufactured in accordance to AWS A5.22 but without a specific classification. Shied-Bright 2509 is usable for UNS S32750 (SAF 2507 and URN47N+2), S32760 (Zeron 100 & FAC100) and J9338380 (cast Zeron 100) and similar compositions. It is also suitable for the welding of Ferralium® UNS S32550 and CD-4MCu except for applications where sulfuric or sulfurous acids are present, such as scrubbers for power plants.
Shield-Bright 2509 was developed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.
* This item is subject to Industry Alloy Surcharges

| As Welded 75% Ar / 25% CO2 | |
|---|---|
| Yield Stress | 100 ksi, 690 MPa |
| Tensile Strength | 130 ksi, 900 MPa |
| Elongation in 2" | 28 % |
| V-Notch Impact Toughness | |
| Absorbed Energy @ -40ºF (-40ºC) | 27 ft.-lbs., 37 J |
| Absorbed Energy @ -20ºF (-29ºC) | 32 ft.-lbs., 43 J |
| Typical Undiluted Weld Metal Analysis | |
| 75% Ar / 25% CO2 | |
| C | 0.03 % |
| Mn | 0.9 % |
| Si | 0.6 % |
| Cr | 25 % |
| Ni | 9.7 % |
| Mo | 4 % |
| Cu | 0.1 % |
| N | 0.25 % |
| Ferrite | 45 FN |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 100 A | 23 | 265 ipm, 6.7 cm/min | 2.9 lbs./hr., 1.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 130 A | 25 | 227 ipm, 5.8 cm/min | 4.25 lbs./hr., 1.9 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 165 A | 26 | 341 ipm, 8.7 cm/min | 6.14 lbs./hr., 2.8 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 190 A | 28 | 445 ipm, 11.3 cm/min | 8.08 lbs./hr., 3.7 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 220 A | 30 | 567 ipm, 14.4 cm/min | 10.24 lbs./hr., 4.6 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 170 A | 25 | 154 ipm, 3.9 cm/min | 5.34 lbs./hr., 2.4 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 210 A | 27 | 193 ipm, 4.9 cm/min | 6.89 lbs./hr., 3.1 kg./hr. | 82.5 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 250 A | 28 | 243 ipm, 6.2 cm/min | 8.57 lbs./hr., 3.9 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 29 | 321 ipm, 8.2 cm/min | 11.43 lbs./hr., 5.2 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2