Spoolarc 65 is a triple deoxidize (Aluminum, Titanium, Zirconium) GMAW/GTAW welding wire. It's sluggish puddle makes it suitable for out of position welding. Spoolarc 65 produces extremely good impact properties using the GTAW process.
Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.
Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.
Spoolarc 85 contains moderate levels of deoxidizers and is suitable for many general purpose carbon steel MIG applications. Spoolarc 85 can be used over light rust or light mill scale.
Spoolarc 86 contains higher levels of manganese and silicon than other grades of MIG wire. It provides a highly fluid puddle and excellent tolerance of rust and scale.
Spoolarc 87 HP features an optimized manganese to silicon ratio. It is suitable for welding over moderate amounts of rust and scale.
Spoolarc Easy Grind is a fully deoxidized wire designed to weld over the moderate levels of rust and paint commonly encountered in auto body repair work.
Spoolarc 53 is designed for single or multipass welding on carbon and low alloy steels. It provides higher strength deposits and good impact toughness.
Spoolarac 80 is a low manganese and silicon wire. It provides excellent ductility and crack resistance. Typical applications include lap welds, build-up, or repair welding prior to machining.
Spoolarc 81 is a medium manganese and silicon wire with nominal rust and mill scale tolerance. Typical applications include structural steels, medium strength pressure vessels, ship, barge, and offshore oil rig fabrication.
Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as-welded and stress-relieved conditions. Spoolarc 83 is typically used on heavy equipment and high strength piping.
Spoolarc 40B is a 1/2% Mo containing submerged arc wire most commonly used for stress relief applications.
Spoolarc 40 is a submerged arc wire that is typically used to weld carbon and low alloy steels. It contains 1/2% Mo and elevated levels of Mn which make it suitable for stress relieved applications requiring 80 ksi tensile strength.
Spoolarc 95 is Military grade high strength wire used to weld HY-80 steels. Applications for Spoolarc 95 include military tanks, ships and submarines.
Spoolarc 120 is designed to weld high strength, quenched and tempered steels.
Spoolarc 140 is a high strength wire designed to weld HY-130 steels.
Spoolarc 44 is a high Mn, 1/2% Mo wire with a 0.6% Ni addition designed for single or multipass welding where high strength and impact toughness are required. It maintains 80 ksi after long-term, 50 hours or more, stress relieving.
Spoolarc 100 is a Cr, Ni, Mo alloyed submerged arc welding wire suitable for welding of high strength, low alloy quenched and tempered steels.
Spoolarc U515 is a submerged arc wire that is used for welding Cr-Mo steels up to 1-1/4% Cr and 1/2% Mo. Typical applications include process piping, heat exchangers, and pressure vessel fabrication.
Spoolarc 75 is a MIG and submerged arc wire with 1% nickel content that meets the weathering requirements of AWS D1.1 and D1.5.
Spoolarc WS is an ER80S-G special purpose wire designed to weld "weathering" grade steels.
Spoolarc ENi4 is a submerged arc welding wier that contains 1.7% Ni and 0.15% Mo. It is typically used for the welding of high-strength, low alloyed steels where higher strength and good notch toughness are required.
Spoolarc 71 is a medium manganese and silicon subarc wire that has been microalloyed with titanium. It will produce a minimum 70 ksi tensile strength as welded or after 8 hours stress relief.
Spoolarc 36 is a high manganese wire for single or multipass welding. Typical applications include seam welding on hot water tanks, valves, fittings, and heavy vessel fabrication.