Print this page

SPOOLARC 29S

Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.

Features

Spoolarc 29S is a general purpose copper-coated solid wire suitable for many carbon steel welding applications using either the MIG/Gas Metal Arc Welding (GMAW) or the Submerged Arc Welding (SAW) processes. Spoolarc 29S contains moderate amounts of manganese and silicon to provide sufficient deoxidation over light mill scale. Shielding gas choices for Spoolarc 29S in the GMAW mode are 100% carbon dioxide, argon/carbon dioxide mixtures, argon/oxygen mixtures, and other argon based mixed gas blends. In the SAW mode, Spoolarc 29S can be combined with a variety of active and neutral bonded fluxes to achieve better welding performance over Spoolarc 81 wire. Spoolarc 29S is used in a wide variety of applications including heavy equipment, automotive parts, railcars, agricultural equipment, and sheet metal welding.

Spoolarc 29S
  • Industry
  • Civil Construction
  • Automotive
  • Mobile Machinery
  • General Fabrication
  • Welding Process
  • SAW (Sub Arc)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA5.18; ER70S-3
    • Certified by CWB to CSA W48
    • CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3)
    • AWS.ASME SFA5.17; EM13K
    • ABS 3SA, 3YSA

Properties

Typical Properties
As Welded GMAW CO2  
Yield Strength 61 ksi, 420 MPa
Tensile Strength 73 ksi, 505 MPa
Elongation in 2" 32 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0°F (-18°C)  
As Welded GMAW CO2 95 ft.-lbs., 129 J
Typical Undiluted Weld Metal Analysis  
GMAW CO2  
C 0.07 %
Mn 0.8 %
Si 0.3 %
P 0.009 %
S 0.009 %
Typical Wire Analysis  
C 0.08 %
Mn 1.2 %
Si 0.6 %
P 0.007 %
S 0.007 %
Cu 0.07 %
Wire Chemistries  
C 0.09 %
Mn 1.10 %
Si 0.52 %
P 0.008 %
S 0.012 %

SAW

Accessories

Depositions

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.

Extra Info