Print this page

SPOOLARC 85

Spoolarc 85 contains moderate levels of deoxidizers and is suitable for many general purpose carbon steel MIG applications. Spoolarc 85 can be used over light rust or light mill scale.

Features

Spoolarc 85 contains more manganese and silicon for greater deoxidation capability when compared to ER70S-3 wire. The higher level of deoxidizers provides for better rust and scale tolerance and it also improves bead wetting. Spoolarc 85 is typically used for applications including welding of farm machinery, material handling equipment, and piping.

Spoolarc 85
  • Industry
  • Shipbuilding
  • General Fabrication
  • Automotive
  • Mobile Machinery
  • Welding Process
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • A.B.S. ER70S-4H4

Properties

Typical Properties
As Welded GMAW 98% Ar / 2% O2  
Yield Strength 69 ksi, 475 MPa
Tensile Strength 83 ksi, 570 MPa
Elongation in 2" 25 %
As Welded GMAW CO2  
Yield Strength 65 ksi, 450 MPa
Tensile Strength 78 ksi, 545 MPa
Elongation in 2" 26 %
Typical Undiluted Weld Metal Analysis  
GMAW CO2  
C 0.09 %
Mn 1.0 %
Si 0.5 %
P 0.011 %
S 0.010 %
GMAW 98% Ar / 2% O2  
C 0.08 %
Mn 1.1 %
Si 0.6 %
P 0.011 %
S 0.012 %
Typical Wire Analysis  
C 0.08 %
Mn 1.2 %
Si 0.7 %
P 0.008 %
S 0.007 %
Cu 0.1 %

SAW

Accessories

Depositions

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.

Extra Info