Print this page

Spoolarc Easy Grind

Spoolarc Easy Grind is a fully deoxidized wire designed to weld over the moderate levels of rust and paint commonly encountered in auto body repair work.

Features

Spoolarc Easy Grind is a fully deoxidized wire designed to weld over moderate levels of rust and paint as are commonly encountered in auto body repair work. Easy Grind produces welds that easily exceed the tensile requirements of ER70S class wires.
Easy Grind is produced in small diameters and are appropriate for the low current welding machines commonly used in body shops.

Easy Grind
  • Welding Process
  • GMAW (MIG)

Classifications

Properties

Typical Properties
As Welded GMAW 75% Ar / 25% CO2  
Yield Strength 72 ksi, 495 MPa
Tensile Strength 80 ksi, 550 MPa
Elongation in 2" 24 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (-29°C)  
As Welded GMAW 75% Ar / 25% CO2 40 ft.-lbs., 54 J

SAW

Accessories

Depositions

Spray Transfer Welding Parameters
Diameter Electrode Unit Length/Wt Amps Volts Wire Feed Speed Optimum Amps Optimum Volts Optimum Wire Feed Speed
0.023 in, 0.6 mm 8505 in/lb, 476 m/kg 45-90 14-16 150-380 ipm, 381-965 cm/min 70 15 300 ipm, 762 cm/min
0.030 in, 0.8 mm 5000 in/lb, 280 m/kg 60-140 14-16 150-350 ipm, 381-889 cm/min 100 15 220 ipm, 559 cm/min
0.035 in, 0.9 mm 3670 in/lb, 206 m/kg 90-160 15-19 180-300 ipm, 457-762 cm/min 130 17 250 ipm, 635 cm/min
0.045 in, 1.2 mm 2220 in/lb, 124 m/kg 130-200 17-19 125-200 ipm, 318-508 cm/min 160 18 150 ipm, 381 cm/min
0.052 in, 1.4 mm 1665 in/lb, 93 m/kg 150-200 17-20 135-190 ipm, 343-483 cm/min 160 18 140 ipm, 356 cm/min
0.062 in, 1.6 mm 1150 in/lb, 64 m/kg 290-400 26-36 180-280 ipm, 457-711 cm/min 340 27 200 ipm, 508 cm/min